Use 150°C for indium bonding and 250°C for elastomer bonding.
Use 150°C for indium bonding and 250°C for elastomer bonding.
Stanford Advanced Materials (SAM) Corporation is a global supplier of various sputtering targets such as metals, alloys, oxides, ceramic materials. It was first established in 1994 to begin supplying high-quality rare-earth products to assist our customers in the research and development (R&D) fields.